1984ECS Proceedings VolumesOpen access

Nitrite Molten Salt for use in Intermediate Temperature Lithium Cells

J. Poris

Open full text 1 citations

Abstract

The LiNO 2 -KNO 2 (40–60 m/o) molten salt, which melts at 120°C, has been employed as an electrolyte in intermediate temperature lithium cells. The behavior of solid lithium in this electrolyte is analogous to the behavior of lithium in the similar intermediate temperature alkali nitrate electrolyte. Lithium reacts with the melt to form a thin, lithium ion conducting, protective layer which is believed to be Li 2 O. The electrolyte is electrochemically reduced below 1.9 volts versus Li + /Li, and is oxidized to lithium metal and NO 2 gas above 3.5 volts versus Li + /Li. This electrolyte can be used in secondary cells with lithium or high lithium activity negative electrodes, and lower lithium activity positive electrodes which react reversibly with lithium. The resistance of the protective layer on lithium increases with time as the thickness increases. Its resistance is of the order of 1–10 ohms after 10 hours at 150° C.

Open-access reader

About this research paper

What this paper is about

The LiNO 2 -KNO 2 (40–60 m/o) molten salt, which melts at 120°C, has been employed as an electrolyte in intermediate temperature lithium cells. The behavior of solid lithium in this electrolyte is analogous to the behavior of lithium in the similar intermediate temperature alkali nitrate electrolyte. Lithium reacts with the melt to form a thin, lithium ion conducting, protective layer which is believed to be Li 2 O. The electrolyte is electrochemically reduced below 1.9 volts versus Li + /Li, and is oxidized to lithium metal and NO 2 gas above 3.5 volts versus Li + /Li. This electrolyte can be used in secondary cells with lithium or high lithium activity negative electrodes, and lower lithium activity positive electrodes which react reversibly with lithium. The resistance of the protective layer on lithium increases with time as the thickness increases. Its resistance is of the order of 1–10 ohms after 10 hours at 150° C.

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The LiNO 2 -KNO 2 (40–60 m/o) molten salt, which melts at 120°C, has been employed as an electrolyte in intermediate temperature lithium cells. The behavior of solid lithium in this electrolyte is analogous to the behavior of lithium in the similar intermediate temperature alkali nitrate electrolyte. Lithium reacts with the melt to form a thin, lithium ion conducting, protective layer which is believed to be Li 2 O. The electrolyte is electrochemically reduced below 1.9 volts versus Li + /Li, and is oxidized to lithium metal and NO 2 gas above 3.5 volts versus Li + /Li. This electrolyte can be used in secondary cells with lithium or high lithium activity negative electrodes, and lower lithium activity positive electrodes which react reversibly with lithium. The resistance of the protective layer on lithium increases with time as the thickness increases. Its resistance is of the order of 1–10 ohms after 10 hours at 150° C.

Key concepts: Electrolyte, Lithium (medication), Lithium nitrate, Alkali metal, Inorganic chemistry, Molten salt, Salt (chemistry), Chemistry

Related papers

Back to paper searchBrowse research topicsOriginal source
Nitrite Molten Salt for use in Intermediate Temperature Lithium Cells — Research Paper | ScholarLens