2004AIP conference proceedingsOpen access

Shock Sensitivity of LX-04 Containing Delta Phase HMX at Elevated Temperatures

P. A. Urtiew

Open full text 32 citations

Abstract

LX‐04 is a widely used HMX‐based plastic bonded explosive, which contains 85 weight % HMX and 15 weight % Viton binder. The sensitivity of LX‐04 to a single stimulus such as heat, impact, and shock has been previously studied. However, hazard scenarios can involve multiple stimuli, such as heating to temperatures close to thermal explosion conditions followed by fragment impact, producing a shock in the hot explosive. The sensitivity of HMX at elevated temperatures is further complicated by the beta to delta solid‐state phase transition, which occurs at approximately 165°C. This paper presents the results of shock initiation experiments conducted with LX‐04 preheated to 190°C, as well as density measurements and small scale safety test results of the δ phase HMX at room temperature. This work shows that LX‐04 at 190°C is more shock sensitive than LX‐04 at 150°C or 170°C due to the volume increase during the β to δ solid phase transition, which creates more hot spots, and the faster growth of reaction during shock compression.

Open-access reader

About this research paper

What this paper is about

LX‐04 is a widely used HMX‐based plastic bonded explosive, which contains 85 weight % HMX and 15 weight % Viton binder. The sensitivity of LX‐04 to a single stimulus such as heat, impact, and shock has been previously studied. However, hazard scenarios can involve multiple stimuli, such as heating to temperatures close to thermal explosion conditions followed by fragment impact, producing a shock in the hot explosive. The sensitivity of HMX at elevated temperatures is further complicated by the beta to delta solid‐state phase transition, which occurs at approximately 165°C. This paper presents the results of shock initiation experiments conducted with LX‐04 preheated to 190°C, as well as density measurements and small scale safety test results of the δ phase HMX at room temperature. This work shows that LX‐04 at 190°C is more shock sensitive than LX‐04 at 150°C or 170°C due to the volume increase during the β to δ solid phase transition, which creates more hot spots, and the faster growth of reaction during shock compression.

Why it matters

OpenAlex reports 32 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

LX‐04 is a widely used HMX‐based plastic bonded explosive, which contains 85 weight % HMX and 15 weight % Viton binder. The sensitivity of LX‐04 to a single stimulus such as heat, impact, and shock has been previously studied. However, hazard scenarios can involve multiple stimuli, such as heating to temperatures close to thermal explosion conditions followed by fragment impact, producing a shock in the hot explosive. The sensitivity of HMX at elevated temperatures is further complicated by the beta to delta solid‐state phase transition, which occurs at approximately 165°C. This paper presents the results of shock initiation experiments conducted with LX‐04 preheated to 190°C, as well as density measurements and small scale safety test results of the δ phase HMX at room temperature. This work shows that LX‐04 at 190°C is more shock sensitive than LX‐04 at 150°C or 170°C due to the volume increase during the β to δ solid phase transition, which creates more hot spots, and the faster growth of reaction during shock compression.

Key concepts: Explosive material, Materials science, Shock (circulatory), Phase transition, Thermodynamics, Phase (matter), Thermal shock, Composite material