2005Acta Scientiarum Naturalium Universitatis SunyatseniRequires access

Key parameters for low temperature warm compaction of high density iron-based P/M materials

曹顺华, 林信平, 李炯义, 谢湛, 蔡志勇

Open publisher page 1 citations

Abstract

In order to reduce powder temperature to lower than 100 ℃ in warm compaction by changing polymer lubricant design, powder flowability, warm compacting behavior, lubricating mode as well as ultimate tensile strength after sinter-hardening and tempering were investigated systematically. By means of low temperature warm pressing and sintered hardening technique, samples with the sintered densities of 7.40-7.45 g/cm3 and the strengths of 950-1 390 MPa are achieved as the early compacting pressure is 686-735 MPa.

About this research paper

What this paper is about

In order to reduce powder temperature to lower than 100 ℃ in warm compaction by changing polymer lubricant design, powder flowability, warm compacting behavior, lubricating mode as well as ultimate tensile strength after sinter-hardening and tempering were investigated systematically. By means of low temperature warm pressing and sintered hardening technique, samples with the sintered densities of 7.40-7.45 g/cm3 and the strengths of 950-1 390 MPa are achieved as the early compacting pressure is 686-735 MPa.

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

In order to reduce powder temperature to lower than 100 ℃ in warm compaction by changing polymer lubricant design, powder flowability, warm compacting behavior, lubricating mode as well as ultimate tensile strength after sinter-hardening and tempering were investigated systematically. By means of low temperature warm pressing and sintered hardening technique, samples with the sintered densities of 7.40-7.45 g/cm3 and the strengths of 950-1 390 MPa are achieved as the early compacting pressure is 686-735 MPa.

Key concepts: Compaction, Materials science, Lubricant, Tempering, Hardening (computing), Ultimate tensile strength, Composite material, Pressing